  修補(bǔ)膠是由A和B雙組份構(gòu)成,使用時嚴(yán)格按規(guī)則的合作比將A組份和B組份充沛混合,按質(zhì)量比A:B=7:1或體積比A:B=4:1。并在規(guī)則的可操作時限內(nèi)用完,分配好的膠假如一次性沒用完,此剩下膠不可再使用,主張隨用隨配,降低浪費。
  Repair glue is composed of A and B two components, the use of strictly in accordance with the rules of the cooperation ratio of A and B components fully mixed, according to the mass ratio of A:B = 7:1 or volume ratio of A:B = 4:1. And in the rules can be used up within the operational time limit, if the allocated good glue is not used up at one time, the remaining glue can not be used again, advocate with use with, reduce waste.
  用刮板或膠刀將混合好的修補(bǔ)膠涂于待修外表,可先涂少數(shù),用刮板或膠刀反復(fù)按壓,使修補(bǔ)膠與基體充沛滋潤灌實,隨后再涂剩下的修補(bǔ)膠,留出余量便于加工,或選擇成型法。
  With the scraper or plastic knife will be mixed with good repair glue coated on the appearance of repair, can be first coated with a few, with the scraper or plastic knife repeatedly pressed, so that the repair glue and the matrix full moisture filling, and then coated with the remaining repair glue, leaving a margin for processing, or select the molding method.
  固化必定時刻后就可以選擇傳統(tǒng)的機(jī)加工辦法車削、磨削、鉆孔、攻絲等,以到達(dá)請求尺度;固化后如不需機(jī)加工,可以在施膠外表固化前,用手掌沾少數(shù)水抹平外表,以取得光滑的外外表;加工后如看到外表有氣孔,要對氣孔處從頭鉆孔(少2mm深),隨后從頭填料(相同要粗糙化和清潔外表)。
  Curing must be time after you can choose the traditional machining methods turning, grinding, drilling, tapping, etc., to reach the request scale; After curing, if there is no need for machining, you can use the palm of your hand to wipe the surface with a small amount of water before curing the sizing surface, in order to achieve a smooth appearance; After processing, if you see the appearance of pores, you should drill holes from scratch (at least 2mm deep), and then fill them from scratch (the same to rough and clean the appearance)。
  不銹鋼內(nèi)膽實木酒桶的漏洞不僅僅會影響美觀,嚴(yán)重時則會影響其正常的應(yīng)用,所以一旦發(fā)現(xiàn)就要趕緊進(jìn)行修補(bǔ),更多內(nèi)容就來網(wǎng)站www.lmkxbs.cn看看吧!
  The leak of stainless steel liner solid wood wine barrel will not only affect the appearance, serious will affect its normal application, so once found to be quickly repaired, more content to the website www.lmkxbs.cn see it!

咨詢熱線:
0537-4556677

同江市| 洛川县| 个旧市| 安仁县| 宁武县| 会同县| 晋江市| 吉木乃县| 宁化县| 万载县| 丹阳市| 北流市| 南丰县| 伊宁县| 十堰市| 茌平县| 合肥市| 隆林| 长乐市| 宾阳县| 景德镇市| 仁化县| 岗巴县| 舞钢市| 随州市| 北流市| 陵川县| 卢湾区| 翼城县| 南宁市| 临沭县| 和平区| 富阳市| 民乐县| 革吉县| 霍州市| 朝阳市| 黑山县| 湄潭县| 雷波县| 富平县|